Specifications |
Data | |||
|
Grames |
80 |
g/m2 | ||
|
Tolerance |
+(-)2 |
g/m2 | ||
|
Thickness |
110 |
um | ||
|
Brightness |
102-104% |
% | ||
|
CIE Whitness |
160-167 |
% | ||
|
Opacity |
>94 |
% | ||
|
Breaking of Length |
>3200 |
M | ||
|
Smothness |
>22 |
S | ||
|
>20 |
S | |||
|
Water absorption: cabb method |
<30 |
g/m2 | ||
|
Cross hygro instability |
<2.8 |
% | ||
|
Atomy |
80 |
M2 | ||
|
No |
M2 | |||
|
Mositure content |
3.5-4.5 |
% | ||
|
Ash content |
<16.5 |
% | ||
|
Stiffness |
vibration |
Longitudinal |
0.52 |
mN |
|
Lateral |
0.29 | |||
|
bending |
Longitufinal |
>116 |
Mn | |
|
lateral |
>50 | |||
|
Apparent density of paper |
0.71-0.76 |
g/m3 | ||